• JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
 
  Bookmark and Share
 
 
Thèse de Doctorat
DOI
https://doi.org/10.11606/T.85.2006.tde-04062007-152214
Document
Auteur
Nom complet
Carlos Augusto Xavier Santos
Unité de l'USP
Domain de Connaissance
Date de Soutenance
Editeur
São Paulo, 2006
Directeur
Jury
Bressiani, José Carlos (Président)
Castanho, Sonia Regina Homem de Mello
Goldenstein, Helio
Toffoli, Samuel Marcio
Yoshimura, Humberto Naoyuki
Titre en portugais
"Estudo do compósito 3Y-TZP/Sl2N2O obtido por sinterização sem pressão"
Mots-clés en portugais
Carbeto de Silício
Compósito
Nitreto de Silício
Oxinitreto de Silício
Zircônia
Resumé en portugais
Zircônia 3YTZP apresenta propriedades excelentes à temperatura ambiente, mas estas propriedades são afetadas pelo aumento da temperatura pois esta age negativamente sobre o mecanismo de transformação de fase induzida por tensão, que fortalece a tenacidade da matriz. A adição de Si3N4 e SiC em uma matriz de 3YTZP é muito interessante porque conduz à formação de oxinitreto de silício, melhorando as propriedades mecânicas tais como dureza e tenacidade, mas esta adição está limitada por várias dificuldades que se apresentam durante o processamento e sinterização destes materiais. Neste trabalho foi estudada a obtenção, por sinterização sem pressão, do compósito Y-TZP/Si2N2O, partindo-se da adição de 20vol%Si3N4-SiC em uma matriz de zircônia dopada com 3mol% de Y2O3 - 3YTZP, utilizando-se Al2O3 e Y2O3 como aditivos de sinterização. A mistura foi moída e moldada por prensagem isostática a frio. Amostras foram sinterizadas a 1500º, 1600º e 1700ºC por 2h sem pressão e em atmosfera ambiente, utilizando-se um leito de nitreto de silício. Após sinterização, as amostras foram caracterizadas por difração de raios-X. Foram medidas a densidade, tenacidade, dureza e resistência mecânica à flexão em temperatura ambiente. A estrutura do material foi observada em microscopia eletrônica de varredura e de transmissão, com mapeamento químico, para verificar a homogeneidade e morfologia das fases do compósito. A formação de Si2N2O foi observada no material sinterizado devido à reação entre os pós adicionados. O material obtido apresentou aumento de tenacidade e dureza com o aumento de temperatura de sinterização. As amostras apresentaram boa resistência à oxidação a 1000ºC.
Titre en anglais
3Y-TZP/Si2N2O COMPOSITE OBTAINED BY PRESSURELESS SINTERING
Mots-clés en anglais
Carbide
Composite
Nitride
Oxynitride
Zirconia
Resumé en anglais
Zirconia 3YTZP presents excellent properties at room temperature. These properties decrease as the temperature increases because high temperature acts negatively over the stress induced transformation toughening in the matrix. The addition of Si3N4 and SiC in a Y-TZP matrix is very interesting because leads to formation of silicon oxynitride and it increases the mechanical properties like toughness and hardness. Certainly the mechanical properties increment is limited by several difficulties which have appeared during processing and heating of these materials. This paper studies the Y-TZP/Si2N2O pressureless sintered composite, under different temperatures, showing the behavior of 20vol%Si3N4-SiC when added in YTZP matrix and heated under no pressure system. Al2O3 and Y2O3 were used as sintering aids. The mixture was milled and molded by cold isostatic pressure. Samples were heated at 1500º, 1600º and 1700ºC x 2h without pressure under atmospheric conditions using Si3N4 bed-powder. Samples were characterized by XRD and density, hardness, toughness, bending strength were measured. The structure of the material was observed in SEM/TEM/EPMA to verify the distribution and composition of the materials in the composite and the contact between filler surface and the matrix. The formation of SiON2 was observed in the sintered material due to reaction between both nitride and carbide with Y-TZP matrix. Furthermore the material showed an increment of both hardness and toughness as temperature increases. The samples presented considerable resistance to oxidation below 1000ºC.
 
AVERTISSEMENT - Regarde ce document est soumise à votre acceptation des conditions d'utilisation suivantes:
Ce document est uniquement à des fins privées pour la recherche et l'enseignement. Reproduction à des fins commerciales est interdite. Cette droits couvrent l'ensemble des données sur ce document ainsi que son contenu. Toute utilisation ou de copie de ce document, en totalité ou en partie, doit inclure le nom de l'auteur.
Date de Publication
2007-06-22
 
AVERTISSEMENT: Apprenez ce que sont des œvres dérivées cliquant ici.
Tous droits de la thèse/dissertation appartiennent aux auteurs
CeTI-SC/STI
Bibliothèque Numérique de Thèses et Mémoires de l'USP. Copyright © 2001-2024. Tous droits réservés.