• JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
 
  Bookmark and Share
 
 
Mémoire de Maîtrise
DOI
https://doi.org/10.11606/D.3.2017.tde-23022017-110109
Document
Auteur
Nom complet
Paula Aliprandini
Adresse Mail
Unité de l'USP
Domain de Connaissance
Date de Soutenance
Editeur
São Paulo, 2016
Directeur
Jury
Espinosa, Denise Crocce Romano (Président)
Souza, Kellie Provazi de
Torem, Mauricio Leonardo
Titre en portugais
O uso da extração por solventes para tratamento de licor de lixiviação de minério limonítico de níquel.
Mots-clés en portugais
Acorga M5640
Cyanex 272
Extração por solventes
Minério
Precipitação de ferro
Resíduos (Tratamento)
Solventes
Resumé en portugais
O minério limonítico de níquel é considerado uma fonte de níquel e cobalto a partir de mineração. No entanto, o minério é heterogêneo e a concentração dos metais varia conforme a localização. Sendo assim, é necessário o desenvolvimento de uma metodologia que permita determinar os parâmetros de operação de um processo de separação de metais levando em consideração a composição de cada minério. No processo hidrometalúrgico, diversas técnicas de purificação ou separação dos metais podem ser usadas. O presente trabalho estudou o uso da extração por solventes para tratar o licor baseado no lixiviado de minério limonítico de níquel. No processo de extração por solventes foram determinados os parâmetros de extração dos metais como: pH, concentração do extratante na fase orgânica e diluído em querosene, relação entre as fases aquosa e orgânica (A/O) e número de contatos contracorrente teóricos para extração do metal. A extração de 100% do ferro utilizando Cyanex 272 foi determinada em pH 2, concentração do extratante 25% em volume diluído em querosene, relação A/O 1/3 e três contatos contracorrente. Durante a extração do ferro também houve coextração de 27% do cobalto. Foi possível recuperar o cobre da solução através da extração utilizando Acorga M5640 em pH 2, concentração do extratante na fase orgânica igual 5% v/v, relação entre as fases 1/1 e um contato contracorrente. O alumínio e o zinco foram extraídos em pH 3,5, utilizado Cyanex 272 como extratante na concentração 25% em volume, relação A/O 1/2 e dois contatos contracorrente. A fim de obter uma solução aquosa contendo apenas níquel em solução, a última etapa foi a remoção dos metais remanescentes na solução (cobalto, cromo, magnésio e manganês) utilizando Cyanex 272. O pH para essa extração foi 5, a concentração do extratante 20% v/v, relação entre as fases 1/1 e cinco contatos contracorrente. Ao final, foi possível obter uma solução aquosa contendo níquel em solução na concentração 2,52g/L, o que corresponde a 100% do níquel presente na solução sintética. Além do níquel, 0,19 g/L de magnésio e 0,008g/L de cromo permaneceram na solução final.
Titre en anglais
The use of solvent extraction for treatment of leach liquor of nickel limonite ore.
Mots-clés en anglais
Acorga M5640
Cyanex 272
Iron precipitation
Nickel limonite ore
Solvent extraction
Resumé en anglais
Nickel limonite ore is a source of nickel and cobalt. However, the ore is heterogeneous and concentration changes according the location of the ore. Therefore, determination of the operating parameters is required to separate the metals taking into account the composition of these ores. Hydrometallurgical process is used to treat leach liquor from ores. This work studied the treatment of synthetic solution based on leach liquor of nickel limonite ore by solvent extraction. During the study was determinated the metals extraction parameters as pH, extractant concentration in the organic phase, aqueous and organic ratio (A/O) and number of theoretical extraction stages. The extraction of iron was 100% using Cyanex 272 at pH 2, extractant concentration 25% (v/v) and three extraction stages at an A/O ratio 1/3. Nevertheless, during the extraction of iron, cobalt was co-extracted. The cobalt lost was 27% at the parameters used to extract. It was possible to recover copper from the synthetic solution using Acorga M5640 as extractant at pH 2, extractant concentration 5% v/v, one extraction stage and an A/O ratio 1/1. Aluminium and zinc were removed from synthetic solution at pH 3.5, organic phase with 25% v/v of Cyanex 272 and two extraction stages at an A/O ratio 1/2. The last part of work was removed cobalt, chromium, magnesium and manganese from the aqueous solution. The reason is staying just nickel in the final solution. Cyanex 272 at pH 5 and 20% v/v concentration was used and five extraction stages and an A/O ratio 1/1 was necessary to extract the metals. The finally solution was composed by 2.52g/L of nickel, corresponding 100% of nickel from synthetic leach liquor of nickel limonite ore. In addition, 0.19g/L of magnesium and 0.008g/L of chromium staying at solution.
 
AVERTISSEMENT - Regarde ce document est soumise à votre acceptation des conditions d'utilisation suivantes:
Ce document est uniquement à des fins privées pour la recherche et l'enseignement. Reproduction à des fins commerciales est interdite. Cette droits couvrent l'ensemble des données sur ce document ainsi que son contenu. Toute utilisation ou de copie de ce document, en totalité ou en partie, doit inclure le nom de l'auteur.
Date de Publication
2017-02-24
 
AVERTISSEMENT: Apprenez ce que sont des œvres dérivées cliquant ici.
Tous droits de la thèse/dissertation appartiennent aux auteurs
CeTI-SC/STI
Bibliothèque Numérique de Thèses et Mémoires de l'USP. Copyright © 2001-2024. Tous droits réservés.