• JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
 
  Bookmark and Share
 
 
Disertación de Maestría
DOI
https://doi.org/10.11606/D.58.2010.tde-11112010-152455
Documento
Autor
Nombre completo
Renan de Barros e Lima Bueno
Dirección Electrónica
Instituto/Escuela/Facultad
Área de Conocimiento
Fecha de Defensa
Publicación
Ribeirão Preto, 2010
Director
Tribunal
Oliveira, Paulo Tambasco de (Presidente)
Ferreira Júnior, Osny
Garcia Junior, Idelmo Rangel
Título en portugués
Desenvolvimento do fenótipo osteogênico in vitro sobre diferentes nanotopografias de titânio funcionalizadas com o fator de crescimento GDF-5
Palabras clave en portugués
Cultura de células
Fator de crescimento
Funcionalização
Nanotopografia
Osteogênese
Resumen en portugués
Modificações bioquímicas de topografias complexas de Ti permitem o desenvolvimento de novas superfícies de implantes funcionalizadas com moléculas bioativas, visando a promover a osteogênese de contato e a osseointegração. O objetivo do presente estudo foi avaliar o desenvolvimento do fenótipo osteogênico in vitro sobre diferentes nanotopografias de titânio (Ti) funcionalizadas com o fator de crescimento GDF-5. Células osteogênicas derivadas de calvária de ratos recém-nascidos foram plaqueadas e cultivadas por até 14 dias sobre superfícies de discos de Ti: 1) Controle (usinada e polida); 2) 30′ (com nanotopografia de nanoporos menores, obtida por condicionamento em solução de H2SO4/H2O2 por 30 min); 3) 30′+GDF-5 (nanotopografia de 30′, pré-adsorvida com GDF-5 a 200 ng/mL); 4) 4h (com nanotopografia de nanoporos maiores, obtida por condicionamento em H2SO4/H2O2 por 4 h); 5) 4h+GDF-5 (nanotopografia de 4h, pré-adsorvida com GDF-5 a 200 ng/mL). A adsorção de GDF-5 foi realizada a 4 ºC por 12 h no dia anterior ao plaqueamento das células. Os resultados mostraram que não houve diferenças estatisticamente significantes entre os grupos para a viabilidade celular em 1, 3 e 7 dias. Em 3 dias, as células estavam aderidas e espraiadas sobre todas as superfícies e acúmulos extracelulares extensos de OPN foram encontrados apenas sobre superfícies com nanotopografia de 4h e de 30′+GDF-5. A expressão de RNAm para RUNX2 e ALP foi maior em 7 dias se comparada a 10 dias, sendo os menores valores encontrados para o grupo 4h+GDF-5. A expressão de OPN aumentou de 7 para 10 dias, exceto para 30′+GDF-5, que se manteve inalterada. Enquanto que os níveis de RNAm para BSP aumentaram de 7 para 10 dias no Controle, redução significativa foi observada para os demais grupos, exceto para 30′, em que se manteve constante. Culturas crescidas sobre nanotopografias funcionalizadas com GDF-5 exibiram os maiores valores de atividade de ALP em 10 dias e de áreas de matriz mineralizada/acúmulos de cálcio em 14 dias. Em conclusão, a funcionalização de nanotopografias de Ti com GDF-5 pode acelerar e/ou aumentar a expressão do fenótipo osteogênico in vitro.
Título en inglés
Development of the osteogenic phenotype in vitro on titanium surface nanotopographies functionalized with GDF-5
Palabras clave en inglés
Cell culture
Functionalization
Growth factors
Nanotopography
Osteogenesis
Resumen en inglés
Surface functionalization of metallic surfaces with bioactive molecules has been developed aiming to promote specific cellular responses at the biomaterial-tissue interface. The present study evaluated the development of the osteogenic phenotype in vitro on titanium (Ti) surface nanotopographies functionalized with growth and differentiation factor-5 (GDF-5). Osteogenic cells were obtained by enzymatic digestion of newborn rat calvarial bone and grown for periods of up to 14 days on the following Ti disc surfaces: 1) Machined; 2) 30′ Nanotopography created by a mixture of H2SO4/H2O2 for 30 min; 3) 30′+GDF-5 Nanotopography created by a mixture of H2SO4/H2O2 for 30 min and then adsorbed with 200 ng/mL GDF-5 (overnight at 4 °C); 4) 4h Nanotopography created by a mixture of H2SO4/H2O2 for 4 h; 5) 4h+GDF-5 Nanotopography created by a mixture of H2SO4/H2O2 for 4 h and then adsorbed with 200 ng/mL GDF-5 (overnight at 4 °C). At 4 h, nanotopographies adsorbed with GDF-5 exhibited a significantly lower proportion of spread cells. At days 1, 3 and 7 no major differences in terms of cell viability were detected among groups. At day 3, epifluorescence revealed large extracellular OPN accumulation only for 30′+GDF-5, 4h and 4h+GDF-5. Real time PCR analysis showed for GDF-5 groups: i) lower mRNA levels for RUNX2, ALP e BSP at day 10; ii) higher RUNX2 and ALP expression at day 7 compared with day 10, with the lowest levels for 4h+GDF-5; iii) increased OPN levels from day 7 to day 10, except for 30′+GDF-5, which remained unaltered. Cultures grown on nanotopographies adsorbed with GDF-5 exhibited significantly higher values for ALP activity at 10 days and enhanced mineralized matrix formation at day 14. In conclusion, surface functionalization of Ti nanotopographies with GDF-5 can accelerate and/or increase the expression of the osteogenic phenotype in vitro.
 
ADVERTENCIA - La consulta de este documento queda condicionada a la aceptación de las siguientes condiciones de uso:
Este documento es únicamente para usos privados enmarcados en actividades de investigación y docencia. No se autoriza su reproducción con finalidades de lucro. Esta reserva de derechos afecta tanto los datos del documento como a sus contenidos. En la utilización o cita de partes del documento es obligado indicar el nombre de la persona autora.
ME_RENAN_BARROS.pdf (702.30 Kbytes)
Fecha de Publicación
2015-04-13
 
ADVERTENCIA: Aprenda que son los trabajos derivados haciendo clic aquí.
Todos los derechos de la tesis/disertación pertenecen a los autores
CeTI-SC/STI
Biblioteca Digital de Tesis y Disertaciones de la USP. Copyright © 2001-2024. Todos los derechos reservados.