• JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
  • JoomlaWorks Simple Image Rotator
 
  Bookmark and Share
 
 
Disertación de Maestría
DOI
https://doi.org/10.11606/D.58.2012.tde-18092012-155747
Documento
Autor
Nombre completo
Olivia Cherubin Alves
Dirección Electrónica
Instituto/Escuela/Facultad
Área de Conocimiento
Fecha de Defensa
Publicación
Ribeirão Preto, 2012
Director
Tribunal
Oliveira, Paulo Tambasco de (Presidente)
Aguiar, Marcio Cajazeira
Peitl Filho, Oscar
Título en portugués
Análise da diferenciação osteoblástica in vitro sobre superfícies de materiais vítreos e vitrocerâmicos bioativos
Palabras clave en portugués
cultura de células
diferenciação celular
expressão gênica
osteoblastos
vidros bioativos
vitrocerâmicas bioativas
Resumen en portugués
Materiais vítreos e vitrocerâmicos bioativos podem ser usados particulados ou como scaffolds em diferentes tratamentos de defeitos ósseos. Tratamentos térmicos que possibilitam o desenvolvimento de scaffolds a partir de composições de vidros bioativos introduzem fases cristalinas em sua estrutura amorfa com potencial impacto na bioatividade e biocompatibilidade do material. O objetivo do presente estudo foi avaliar, qualitativa e quantitativamente, o desenvolvimento do fenótipo osteogênico de culturas de células osteoblásticas sobre substratos vítreos e vitrocerâmicos bioativos. Células MC3T3-E1 foram cultivadas em condições osteogênicas por períodos de até 21 dias sobre superfícies de Bioglass® 45S5, de duas preparações de vitrocerâmica bioativa e altamente cristalina, Biosilicato® e Biosilicato® para scaffold, e de borosilicato (vidro bioinerte). Foram avaliados, nos períodos de 7, 12 e 21 dias, morfologia celular, formação de matriz mineralizada e expressão de genes relacionados à osteogênese. Os resultados mostraram confluência das culturas sobre as superfícies de vidros e vitrocerâmicas, com progressiva formação de multicamadas celulares. A quantificação de vermelho de Alizarina revelou aumento de mineralização para culturas sobre materiais bioativos, com os maiores valores para Biosilicato® para scaffold. Expressão diferencial de genes foi observada nos 3 períodos de culturas sobre os materiais vítreo e vitrocerâmicos bioativos em comparação ao vidro bioinerte e sobre as vitrocerâmicas em comparação ao vidro bioativo. Os resultados permitem concluir que modificações em aspectos químicos de materiais vítreos e vitrocerâmicos, com efeitos sobre sua bioatividade, resultam em alteração do potencial osteogênico e do perfil de expressão gênica de células osteoblásticas in vitro. A maior atividade osteogênica sobre o Biosilicato® para scaffold permite considerar esse material um potencial candidato para aplicações em defeitos ósseos.
Título en inglés
In vitro osteoblastic differentiation on bioactive glass and glassceramic surfaces
Palabras clave en inglés
bioactive glass
bioactive glass-ceramic
cell culture
cell differentiation
gene expression
osteoblast
Resumen en inglés
Bioactive glasses and glass-ceramics have been used as bone substitutes in either particulate or scaffold forms. Various thermal treatments that allow the development of scaffolds from bioactive glasses may create varied proportions of new crystalline phases in the amorphous phase with a potential impact on the bioactivity and biocompatibility of the material. The aim of the present in vitro study was to qualitatively and quantitatively evaluate the development of the osteogenic phenotype in osteoblastic cell cultures grown on bioactive glass and glass-ceramic surfaces. MC3T3-E1 cells, subclone 14, were cultured under an osteogenic condition for periods of up to 21 days on the following disc surfaces: Bioglass® 45S5 (bioactive glass), Biosilicate® (bioactive glass-ceramic), Biosilicate® as the material for scaffold preparation (Bio-sc, bioactive glass-ceramic), and borosilicate (bioinert glass). At days 7, 12, and 21 post-plating, cell morphology, mineralized matrix formation and the expression profile of genes associated with osteogenesis were evaluated. Epifluorescence of actin cytoskeleton and DAPI DNA stain revealed confluent cell cultures at day 7 for all groups, with progressive cell multilayering formation. The quantitative analysis of Alizarin red-stained cultures at day 21 revealed significantly enhanced mineralization in cultures grown on bioactive materials compared with the ones on borosilicate and the highest absorbance intensities for the Bio-sc group. Differential gene expression profiles were detected at the three time points evaluated in cultures grown on the bioactive materials in comparison with borosilicate, and on the glass-ceramics in comparison with Bioglass® 45S5. From the results presented, it can be concluded that changes in chemical characteristics of glass and glass-ceramic that may have an impact on their bioactivity index can affect the osteogenic potential and the gene expression profile of osteoblastic cells in vitro. The highest osteogenic activity on Bio-sc renders this material a good candidate for bone defect applications.
 
ADVERTENCIA - La consulta de este documento queda condicionada a la aceptación de las siguientes condiciones de uso:
Este documento es únicamente para usos privados enmarcados en actividades de investigación y docencia. No se autoriza su reproducción con finalidades de lucro. Esta reserva de derechos afecta tanto los datos del documento como a sus contenidos. En la utilización o cita de partes del documento es obligado indicar el nombre de la persona autora.
Fecha de Publicación
2012-11-05
 
ADVERTENCIA: Aprenda que son los trabajos derivados haciendo clic aquí.
Todos los derechos de la tesis/disertación pertenecen a los autores
CeTI-SC/STI
Biblioteca Digital de Tesis y Disertaciones de la USP. Copyright © 2001-2024. Todos los derechos reservados.